详细介绍:
镀锌卷R
|
3.0*1000*C
|
sp781-390
|
镀锌卷R
|
0.25*1000*C
|
sp781-390
|
镀锌卷R
|
0.3*1000*C
|
sp781-390
|
镀锌卷R
|
0.3*1200*C
|
sp781-390
|
镀锌卷R
|
2.95*1250*C
|
sp781-390
|
镀锌卷R
|
3.0*1250*C
|
sp781-390
|
镀锌卷R
|
2.5*1250*C
|
sp781-390
|
|
|
|
镀锌卷R
|
1.5*1250*C
|
DX51D+Z120
|
镀锌卷R
|
3.0*1250*C
|
DX51D+Z120
|
镀锌卷R
|
3.0*1250*C
|
DX51D+Z120
|
镀锌卷R
|
1.5*1250*C
|
S350GD+Z120
|
镀锌卷R
|
2.0*1250*C
|
S350GD+Z120
|
|
|
|
镀锌卷R
|
2.0*1000*C
|
DX51D+Z180
|
镀锌卷R
|
0.5*1000*C
|
DX51D+Z180
|
镀锌卷R
|
0.5*1250*C
|
DX51D+Z180
|
镀锌卷R
|
1.5*1250*C
|
DX51D+Z180
|
镀锌卷R
|
2.0*1000*C
|
DX51D+Z180
|
镀锌卷R
|
2.0*1250*C
|
DX51D+Z180
|
镀锌卷R
|
2.5*1250*C
|
DX51D+Z180
|
镀锌卷R
|
3.2*1000*C
|
DX51D+Z180
|
|
|
|
镀锌卷R
|
0.5*1250*C
|
DX51D+Z275
|
镀锌卷R
|
0.6*1250*C
|
DX51D+Z275
|
镀锌卷R
|
0.75*1250*C
|
DX51D+Z275
|
镀锌卷R
|
0.8*1000*C
|
DX51D+Z275
|
镀锌卷R
|
0.8*1250*C
|
DX51D+Z275
|
镀锌卷R
|
0.9*1250*C
|
DX51D+Z275
|
镀锌卷R
|
1.0*1000*C
|
DX51D+Z275
|
镀锌卷R
|
1.0*1250*C
|
DX51D+Z275
|
镀锌卷R
|
1.2*1000*C
|
DX51D+Z275
|
镀锌卷R
|
1.5*1000*C
|
DX51D+Z275
|
镀锌卷R
|
1.5*1250*C
|
DX51D+Z275
|
镀锌卷R
|
1.6*1250*C
|
DX51D+Z275
|
镀锌卷R
|
1.8*1250*C
|
DX51D+Z275
|
镀锌卷R
|
2.0*1250*C
|
DX51D+Z275
|
镀锌卷R
|
2.3*1250*C
|
DX51D+Z275
|
镀锌卷R
|
2.5*1250*C
|
DX51D+Z275
|
镀锌卷R
|
3.0*1250*C
|
DX51D+Z275
|
镀锌是指在金属、合金或者其它材料的表面镀一层锌以起美观、防锈等作用的表面处理技术。主要采用的方法是热镀锌。
锌易溶于酸,也能溶于碱,故称它为两性金属。锌在干燥的空气中几乎不发生变化。在潮湿的空气中,锌表面会生成致密的碱式碳酸锌膜。在含二氧化硫、硫化氢以及海洋性气氛中,锌的耐蚀性较差,尤其在高温高湿含有机酸的气氛里,锌镀层极易被腐蚀。锌的标准电极电位为-0.76V,对钢铁基体来说,锌镀层属于阳极性镀层,它主要用于防止钢铁的腐蚀,其防护性能的优劣与镀层厚度关系甚大。锌镀层经钝化处理、染色或涂覆护光剂后,能显著提高其防护性和装饰性。
|